How do I get pretty TIG welds?
#1
Elite Member
Thread Starter
iTrader: (46)
Join Date: Dec 2007
Location: Nebraska
Posts: 4,729
Total Cats: 166
How do I get pretty TIG welds?
I know that we have a couple of pros here.
I was just curious as to why my TIG welds aren't the pretty irridescent colors. They are functional, but are always dull grey on mild steel or stainless.
Too much heat?
Wrong filler? Too small of a filler rod?
Not enough Argon? Too much? I keep it around 23 cfh.
Too small of a cup letting the argon shield move?
On mild steel I use ER70S-6, copper clad, usually .035 on .060-.125 wall
Stainless I use 309L as I have it left over from my manifold build which was 316 to mild steel.
Machine is a Miller Syncrowave 180.
I was just curious as to why my TIG welds aren't the pretty irridescent colors. They are functional, but are always dull grey on mild steel or stainless.
Too much heat?
Wrong filler? Too small of a filler rod?
Not enough Argon? Too much? I keep it around 23 cfh.
Too small of a cup letting the argon shield move?
On mild steel I use ER70S-6, copper clad, usually .035 on .060-.125 wall
Stainless I use 309L as I have it left over from my manifold build which was 316 to mild steel.
Machine is a Miller Syncrowave 180.
Last edited by Stein; 01-08-2010 at 02:33 PM.
Thread
Thread Starter
Forum
Replies
Last Post
bigmackloud
Miata parts for sale/trade
19
01-08-2021 11:24 AM
StratoBlue1109
Miata parts for sale/trade
21
09-30-2018 01:09 PM